Most boat windscreen replacement jobs start the same way: the screen has gone cloudy, crazed or yellow, or it has cracked out from a fixing hole, and you are squinting through it on the way back to the ramp. The good news is that the frame almost always outlasts the screen. In most cases you do not need a new windscreen assembly, you need a new sheet cut and shaped to fit the frame you already have.
That is the job we do in our Perth workshop. Bring in your old screen, even cracked, and as long as it still holds its shape we copy it in new acrylic or polycarbonate. Every screen is made to order for your boat, and we supply it ready for you or your marine trimmer to fit. Below is how to tell whether yours needs replacing, which material to choose, and what happens once it is on our bench.
Signs your boat windscreen needs replacing
Some damage polishes out. Most of what makes a screen hard to see through does not. Replace it when you see any of these:
- Crazing. A web of fine cracks just under the surface, usually worst around the fixings. It is stress cracking in the plastic and it cannot be polished out, because it is inside the sheet, not on it.
- Yellowing or a milky haze. Years of UV and salt break the surface down. On an older or non UV-stabilised sheet it goes all the way through.
- Cracks running from fixing holes. The classic failure. The sheet expands and contracts with the sun, the fixings hold it tight, and it cracks at the weakest point.
- Deep scratches you can catch a fingernail in. Light scuffs polish out. Deep ones do not, and trying usually leaves a distorted patch that is worse to look through than the scratch.
- Glare and distortion at night. If oncoming lights smear across the screen, the surface is gone.
Any one of these is a visibility problem, and on the water visibility is a safety problem, not a cosmetic one.
The best material for a boat windscreen: acrylic or polycarbonate
Both are used on boats, and they fail in opposite ways. The right choice depends on what your screen has to put up with.
| Cast acrylic (Perspex) | Polycarbonate | |
|---|---|---|
| Clarity | Excellent, and it stays clear in UV for years | Very good when new |
| Scratch resistance | Better | Scratches more easily |
| Impact strength | Good, but it can crack on a hard hit | Far higher, very hard to break |
| UV | Naturally stable | Needs a UV-protected grade outdoors |
| Polishing | Light scratches polish out well | Harder to polish without hazing |
| Best for | Runabout and cruiser windscreens, where clarity matters most | Screens that take knocks, like offshore, work boats and anything that gets stood on |
For most recreational windscreens we recommend cast acrylic sheet. It is clearer, it keeps its clarity in the West Australian sun, and a scuffed acrylic screen can be brought back. Choose polycarbonate sheet when impact is the bigger risk than scratching, and go in knowing it will scratch more easily. Thickness depends on the size of the screen and how well the frame supports it. Our standard is 4.5 to 6 mm. If you want the full property-by-property breakdown, read perspex vs acrylic vs polycarbonate.
Tinted screens cut glare on bright days. We supply screens in clear, green tint and grey tint.
How we make a replacement boat windscreen
A boat windscreen replacement that fits first time comes down to the template. This is our process:
- Your old screen is the pattern. Bring it in, cracked or not. As long as it still holds its shape, we can copy it. Tape a broken one together as best you can, since the outline matters more than the condition.
- No old screen? It depends on the shape. For a flat screen, a cardboard template is enough. A curved screen needs accurate curves, so we either mould off your existing screen or make a new mould, which adds to the cost. We can also work from a drawing, but that adds design and programming time and cost.
- We trace it onto new sheet with the protective film left on, so the new sheet stays scratch-free all the way through the job.
- We cut the shape and finish the edges. If the edges sit inside a metal frame, polishing usually is not needed. If they will be on show, we can polish them for an extra cost.
- We form it to shape. A simple 90 degree bend is done on a strip heater, with the heat applied along the bend line only, so the rest of the screen stays optically clear. Curved screens are formed over a mould.
Fixing holes are best drilled when you fit the screen, so they line up exactly with your frame. We can drill them for you, but we usually recommend drilling them at install. Use a blunt drill bit, go slowly, and make each hole slightly oversized so the screen can move as it heats and cools. Holes drilled tight are a common reason screens crack at the fixings.
We supply the screen only, with its film still on, and we do not fit it. A flat screen usually takes 7 to 10 business days. Curved screens take 2 to 4 weeks, because the mould has to be made first, and anything thicker than our standard 4.5 to 6 mm can take longer.
Get a boat windscreen quote
Replacing perspex boat windows
Side windows go the same way as windscreens. They are usually flat, which makes replacement simpler, since no bending or mould is involved. The same rule applies: bring in the old window, or a template of it, and we copy it.
If you are replacing perspex boat windows on an older boat, it is worth doing the whole set at once. New panels next to old ones make the old ones look worse, and they will all have had the same years of sun.
Hatch lids are a different job. They are usually vacuum formed, and a one-off replacement is rarely worth the cost, so it is not something we usually take on.
A note on frames. We make the clear panels only. We do not make or repair the aluminium frames they sit in, and we do not install the screens. If your frame is bent or corroded, get that sorted by a marine fabricator first, because a new screen will not straighten a twisted frame, and a twisted frame will crack a new screen.
“Perfect fit first time and look great.”
Nick Cox, BCJ customer, on his new boat windows
Boat windscreen repair: what can and cannot be fixed
Before you pay for a boat windscreen replacement, it is worth knowing what a repair can do.
Can be fixed: light scratches and scuffs on acrylic, and dullness from salt and cleaning. A proper acrylic scratch remover will bring these back. We stock acrylic scratch removers and cleaners for exactly this.
Cannot be fixed: crazing, cracks, deep gouges and through-sheet yellowing. Crazing and yellowing are inside the material. Cracks can be stop-drilled to slow them down, but that is a get-you-home fix, not a repair, and the screen is weaker from then on.
Whatever you do, keep household glass cleaner off it. Cleaners with ammonia or alcohol attack acrylic and are one of the common causes of crazing. Use fresh water, a soft cloth and a cleaner made for acrylic.
Boat windscreen replacement questions
Still deciding? These are the questions boat owners ask most. To see screens we have made, look at our boat windscreen projects, or read more about our boat windscreens and marine parts in Perth.
It depends on the size of the screen, the material, the thickness and whether it is flat or curved. A flat side window costs far less than a large curved windscreen, especially one that needs a new mould. Polished edges are an optional extra. Bring in your old screen, or send us a photo with rough measurements, and we will give you a price. Replacing just the screen is almost always cheaper than replacing the whole windscreen assembly with its frame.
Remove the old screen from the frame, keeping every fixing and noting where each one came from. Have a new screen made using the old one as the template. Drill the fixing holes to match the frame, slowly, with a blunt bit, and slightly oversized. Fit it with new seals or gasket, and do the fixings up snug but not tight so the sheet can move with temperature. We supply the screen only, so you fit it yourself or have a marine trimmer do it.
It depends on the size of the screen and how much of its edge the frame supports. A small, fully framed screen can be thinner than a large, partly frameless one. Our standard is 4.5 to 6 mm, and we will match or improve on your original. Thicker sheet is possible but adds to the turnaround.
Yes. Tinted acrylic cuts glare and heat on bright days. We supply green tint and grey tint, as well as clear. Tint is part of the sheet, not a film applied on top, so it will not peel or bubble.
Rinse the salt off with fresh water first, then wipe with a soft microfibre cloth and a cleaner made for acrylic. Never wipe a dry, salty screen, as the salt crystals scratch it. Avoid household glass cleaners, since ammonia and alcohol cause crazing, and never use paper towel.
A flat screen usually takes 7 to 10 business days. Curved screens take 2 to 4 weeks, because the mould has to be made first, and sheet thicker than our standard 4.5 to 6 mm can add time. If you are working to a launch date, tell us when you bring the old screen in.
Get a quote for your replacement windscreen
Attach a photo of your old screen with rough width and height measurements, and we will come back with a price. If you are in Perth, you are welcome to bring the screen in.
"*" indicates required fields
Get in touch with us
Monday – Thursday: 8am – 4pm
Friday: 8am – 2pm
Saturday – Sunday (closed)
Glue for Acrylic and Perspex: Which One to Use
Read article
How to Cut Polycarbonate Sheet Without Melting the Edge
Read article